Digital Radiography (CR & DDA) Image Quality & Flaw Sizing Guide
Field Procedure for ASME Section V Article 2 & ISO 17636-2 Compliance
Key Technical Takeaways & Execution Rules
- Basic spatial resolution (SR_b) must be verified using a duplex wire gauge per EN ISO 19232-5 to ensure the system resolves required flaw tip dimensions.
- Signal-to-Noise Ratio (SNR) normalization per ISO 17636-2 Class B requires minimum normalized SNR_N >= 100 for high-integrity weld inspections.
- Geometric unsharpness formula: U_g = (f * b) / a, where f = focal spot size, b = object-to-detector distance, and a = source-to-object distance. U_g must not exceed ASME limits (e.g. 0.51mm for t < 50mm).
- Image processing filters (edge enhancement, high-pass filters) must not induce ringing artifacts that mimic root crack indications.
Step-by-Step Field Execution Procedure
Detector Calibration & Bad Pixel Mapping
Perform dark current offset and flat-field gain correction on the DDA panel. Map and mask defective pixel clusters per ASTM E2597.
Exposure Geometry & Unsharpness Setup
Position isotope source (Ir-192, Se-75) or X-ray tube to minimize object-to-detector distance (ODD). Calculate source-to-detector distance (SDD) to satisfy ASME U_g limits.
IQI Placement & Contrast Sensitivity Verification
Place wire-type IQI (ASTM 1B or ISO 10-16) and duplex wire gauge on source-side weld face. Confirm required wire diameter is distinctly visible across 3 consecutive scans.
Digital Acquisition & SNR_N Measurement
Expose panel and acquire raw 16-bit DICONDE image. Sample gray values across weld root and parent metal to verify normalized SNR_N satisfies code threshold.
Flaw Characterization & Archival
Size planar and volumetric weld flaws using calibrated pixel cursors. Export uncompressed DICONDE format with tamper-proof Level III digital signatures.
Governing Physical & Code Formulas
Geometric Unsharpness Limit
Code FormulaCalculates focal spot penumbra blurring to ensure it does not exceed ASME Section V Article 2 limits (e.g. max 0.51mm for t < 50mm).
Probe & Wedge Selection Specs
- High-Resolution CMOS DDA Panel
- Amorphous Silicon TFT DDA Flat Panel
- Flexible Phosphor Storage Screen (CR)
Code Acceptance Criteria
ASME Sec VIII Div 1 UW-51 / ISO 10675-1 Class 1: Any crack, lack of fusion, or incomplete penetration is strictly unacceptable. Porosity clusters and slag evaluated against thickness-dependent length charts.